至(zhi)今(jin)為止,天然真石漆已被廣(guang)大消費者所選用,用的人多,隨著質量問題也就跟(gen)過來了,今天(tian)超前(qian)真(zhen)石漆(qi)廠家就為(wei)大家說說天(tian)然真(zhen)石漆(qi)施工后墻面(mian)露底原(yuan)因及解(jie)決方案:
超前涂料技術人員(yuan)說其(qi)實天然真石漆施工(gong)(gong)后墻面(mian)露底與施工(gong)(gong)有著(zhu)很(hen)大關系,露底原因有好多種,比(bi)如施工(gong)(gong)過程中(zhong)為增(zeng)加用量過度兌水導至涂漠厚度不足,施工(gong)(gong)時噴(pen)涂又不均勻,或者陰陽角局部(bu)地(di)方漏涂;對于以上因施工墻面出現(xian)露底現(xian)象給出解(jie)決方案:施工時(shi)如(ru)涂料過(guo)稠應該(gai)適(shi)當(dang)兌(dui)水,在試板中(zhong)進行(xing)試噴(pen),試(shi)噴到合格為止(zhi)再進行(xing)上墻噴涂(tu),噴涂(tu)前應把(ba)槍的氣(qi)壓及槍的口徑調好,確保(bao)施(shi)(shi)工(gong)時噴灑均(jun)勻,切記不要(yao)在過低的吸水率基面進行(xing)噴涂(tu),噴涂(tu)施(shi)(shi)工(gong)時監理應加強施(shi)(shi)工(gong)監管,防止(zhi)局部陰陽角漏(lou)涂(tu)。
天然真(zhen)石(shi)漆施工后(hou)要想(xiang)給人呈現出(chu)完美的飾面效果(guo)就必須(xu)有著(zhu)優質的天然真石漆加上(shang)科學(xue)系(xi)統涂(tu)裝(zhuang)工藝(yi)再(zai)加上(shang)好的施工師傅才能做出(chu)完美的工程.